Our sawn timber is sorted according to quality and left in a shaded area for natural drying, reducing its moisture content from 90–100% to 30-40%. After reaching this moisture level, the kiln drying process begins. This process is computer-assisted, achieving a moisture content of 8-12%, after which the timber can be used in the manufacturing of furniture, stairs, countertops, etc.
Standard quality is recommended for those areas where economic efficiency is a priority. It is ideal for making stairs, doors, long elements, etc.
1-2 sound knots, end cracks as wide as the width of the piece and mirrors are acceptable.