Our sawn timber is sorted according to quality and left in a shaded area for natural drying, reducing its moisture content from 90–100% to 30-40%. After reaching this moisture level, the kiln drying process begins. This process is computer-assisted, achieving a moisture content of 8-12%, after which the timber can be used in the manufacturing of furniture, stairs, countertops, etc.
This quality accepts a higher percentage of sapwood, multiple healthy knots, end cracks twice the width of the piece. Vicious knots larger than 30 mm in diameter, the actual heart and the clogged shell are rehabilitated. Insect holes and rot are not accepted. Density 700 - 750 kg / m3.
Rustic quality accepts multiple healthy knots, end cracks twice the width of the piece. Vicious knots larger than 30 mm in diameter, the actual heart and the clogged bark are rehabilitated. Insect holes and rot are not accepted. Density 720 kg / m3.
It is a hemmed lumber with a uniform yellowish-brownish uniform color. The lumber is predominantly clean, but 1-2 healthy knots and end splits as wide as the width of the piece are acceptable.