Our sawn timber is sorted according to quality and left in a shaded area for natural drying, reducing its moisture content from 90–100% to 30-40%. After reaching this moisture level, the kiln drying process begins. This process is computer-assisted, achieving a moisture content of 8-12%, after which the timber can be used in the manufacturing of furniture, stairs, countertops, etc.
Standard quality beech timber is a predominantly clean timber.
We accept 1-2 sound knots, end cracks as wide as the width of the piece and 10-15% red heart .
Insect holes and rot are not acceptable.
Density 720 kg / m3.