Our sawn timber is sorted according to quality and left in a shaded area for natural drying, reducing its moisture content from 90–100% to 30-40%. After reaching this moisture level, the kiln drying process begins. This process is computer-assisted, achieving a moisture content of 8-12%, after which the timber can be used in the manufacturing of furniture, stairs, countertops, etc.
Este o cherestea tivita, cu o culoare uniforma galbui maronie.
Cheresteaua este preponderent curata, dar sunt acceptate 1-2 noduri sanatoase si crapaturile de capat cat latimea piesei.