Our sawn timber is sorted according to quality and left in a shaded area for natural drying, reducing its moisture content from 90–100% to 30-40%. After reaching this moisture level, the kiln drying process begins. This process is computer-assisted, achieving a moisture content of 8-12%, after which the timber can be used in the manufacturing of furniture, stairs, countertops, etc.
Este o cherestea tivita, cu o culoare uniforma galbui maronie.
Cheresteaua este preponderent curata, dar sunt acceptate 1-2 noduri sanatoase si crapaturile de capat cat latimea piesei.
Aceasta calitate accepta un procent mai mare de alburn, noduri sanatoase multiple, crapaturi de capat de doua ori cat latimea piesei.
Nodurile vicioase mai mari de 30 mm in diametru, inima propriu zisa si coaja infundata se bonifica .
Nu se accepta gauri de insecte, si putregai.
Densitate 700 - 750 kg / m3.