Our sawn timber is sorted according to quality and left in a shaded area for natural drying, reducing its moisture content from 90–100% to 30-40%. After reaching this moisture level, the kiln drying process begins. This process is computer-assisted, achieving a moisture content of 8-12%, after which the timber can be used in the manufacturing of furniture, stairs, countertops, etc.
Cheresteaua de fag calitate standard, este o cherestea preponderent curata.
Se accepta 1-2 noduri sanatoase, crapaturi de capat cat latimea piesei si inima rosie in proportie 10-15 .
Nu se accepta gauri de insecte, si putregai.
Densitate 720 kg / m3.